GB/T 3077 42CrMo4 alloy steel

Hardness: <=217HBW
Thermal processing Temperature1050-850
Heat Treatment: Annealed: 680-720°C
Normalized: 840-880°C
Quenched: 820-850°Cfor water, 830-860°C for oil
Tempered: 540-680°C

42CrMo4 alloy steel Chemical composition %:

C

Si

Mn

P

S

Cr

Mo

0.38- 0.45

max   0.4

0.6 - 0.9

max   0.025

max   0.035

0.9 - 1.2

0.15 - 0.3

GB/T 3077 42CrMo4 Mechanical properties:

Yield
Rp0.2 (MPa)

Tensile
Rm (MPa)

Impact
KV/Ku (J)

Elongation
A (%)

252 (≥)

877 (≥)

24

14

GB/T 3077 42CrMo4 Applications:
To manufacture high strength and conditioning section part that request more than 35CrMo, such as locomotive traction gear, supercharger gear. Connecting rod and spring clip, can also be used for oil drill pipe joints below 2000m deep.

Get Latest Price

We guarantee that your information will not be divulged to third parties and reply to you within 24 hours.

If you need the latest price list, please leave us a message here, thank you! We guarantee that your information will not be divulged to third parties and reply to you within 24 hours.

  • Your Email
  • Your Name
  • Requirements( as specific as possible )

Hot Products

Last Post